Monday, December 31, 2012

Re: [MW:16386] Vacuum Packed LH Electrodes

dear friend,

as per my opinion, it must be placed in site quiver at 120C because vaccum pack replaces the requirement of rebaking not holding. 

wat manufacturer is written 9 hrs.is regarding max. working time before rebaking requries.



On Sun, Dec 30, 2012 at 8:47 AM, ABHISHEK GHOSH <ghoshabhishekmech@gmail.com> wrote:
Dear Experts, 

We are using E 7018-1 H4 Vacuum packed Electrodes for our project. ( Refer attachments ) , where manufacturer recommendations is mentioned as : 
HD [ ml/100g] : at opening time : <5 
Working time after opening : 9h at 80% RH / 27 deg C 
After this period rebaking : 2h/340-360 deg C 
Brand : Supercito VP Medium ,Oerlikon , Air Liquide Wedling France. 
Weather Condition at site : 78- 80 % Humidity , Temp 26-30 Deg C. 

My question is :
  •  After opening packet at the start of the days work , is it necessary to transfer a pack of  electrodes to a portable quiver for holding at temp 100 deg C to prevent further moisture pick up ? or it is not required as manufacturer says that after opening up to 9 hrs it can be used at 80% / 27 deg C . 

  • Electrodes rebaking cycle depends upon which factors? Some client specifies recycling 1 time  , some 2 times ... [ As per BIS 13851:1993 , ( R 2006) - Storage & redrying of coverd electrodes  before use recommendations- 3 times ] 

Please clarify . 

Thanks & regards. 

Abhishek Ghosh 
Indonesia 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...