Hi, Chandra
Normal Industrial Practise- Min 4 x pipe thk. or 100mm whichever greater
Normally it dictated ny Client Spec. or in Engineering Dwgs.
I dont think so codes dictates that.
Hope i'm correct
Welcome more inputs as this question often raised
Thank and With Warmest Regards
Ganesan
Date: Tue, 25 Dec 2012 23:37:06 -0800
From: bocant_btm@yahoo.com
Subject: [MW:16330] minimum length of pipe in the subsea spool..
To: materials-welding@googlegroups.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Normal Industrial Practise- Min 4 x pipe thk. or 100mm whichever greater
Normally it dictated ny Client Spec. or in Engineering Dwgs.
I dont think so codes dictates that.
Hope i'm correct
Welcome more inputs as this question often raised
Thank and With Warmest Regards
Ganesan
Date: Tue, 25 Dec 2012 23:37:06 -0800
From: bocant_btm@yahoo.com
Subject: [MW:16330] minimum length of pipe in the subsea spool..
To: materials-welding@googlegroups.com
deat expert,
i want to ask about,how length minimum of the pipe if any additional joint in the subsea pipe/pipeline.
i try to search in the ASME B31.8 and other spec about pipeline, i dont find minimum length of pipe/distance between weld to weld.
can somebody advise for me,where the spec will be use?!
Thanks for your time and attention.
Regards,
Chandra Putra
Skype: chandra.putra12
Chandra Putra
Skype: chandra.putra12
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments