Skip to main content

Re: RE: [MW:10838] Impact testing temp. for EN19 steel

Hi Babu

Thanks for your reply.
However my second query is unadressed.

"Secondly i would also like to know which of the two will have more toughness and why - EN 19 casting OR EN19 plate ?"

I feel that plate will have more toughness than casting, but how much ???

Can anyone reply to this please ??

Regards

Prem Nautiyal




On Fri, 22 Apr 2011 21:47:03 +0530 wrote
>




















Hello !



Please can someone answer my general
query>



Why only Charpy V Notch Testing is mostly
used for Impact Testing & why Izod is not popular.



Please give detailed information to
understand process thoroughly.



Waiting for replies!





Regards,

Manmeet
Magdum

Document Quality Control – Drilling Riser Systems

QS Supply Chain.

AkerSolutions



( (Tel ) +91-20-66918751

Ë (Mobile)
+91 9762446730

* (Email) Magdum.Manmmet@akersolutions.com

Aker Powergas Subsea Pvt Ltd

BlueRidge , IT-2, Flagship Infrastructure Pvt
Ltd, Ist Floor, Hinjewadi, Pune 411045, India

Registered in India
; CIN;U74990MH2010PTC210736













From:
materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu

Sent: Thursday, April 21, 2011 5:47 AM

To:
materials-welding@googlegroups.com

Subject: Re: [MW:10765] Impact
testing temp. for EN19 steel







Hi











Izod will be done at Room temp., Unless otherwise
specifically mentioned by spec.











Thanks & Regards,











K. Babu







----- Original Message -----





From: PREM
SHANKARDUTT NAUTIYAL





To: materials-welding@googlegroups.com






Sent: Wednesday, April 20, 2011 11:21 PM





Subject: [MW:10758] Impact
testing temp. for EN19 steel









Dear Friends



I wanted to use EN 19 plate in one of my present project, wherein the
application demands severe impact loads at room temperature.



I had browsed through the properties of EN 19 plate in various literatures
wherein the Izod test values are mentioned @ 55J.



However the Izod testing temperature is not mentioned.



Can anyone help me out or guide me where to refer, so that i can know the Izod
testing temperature of this EN 19 steel.



Secondly i would also like to know which of the two will have more toughness
and why - EN 19 casting OR EN19 plate ?

The reason being the final component will have to be casted due geometrical
complications.





Regards



Prem Nautiyal





PREM S NAUTIYAL

CELL : 9769316004









--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.





This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.





--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...