 During review of RT films for a welded joint, linear indication of length 12 mm was observed in HAZ area in Base Metal.  

As the defect was observed in base metal, UT was performed. UT shows 8mm length of indication. UT was carried out by TR Probe. If we perform UT by normal probe no indication is detected.

UT is showing the depth of indication at junction of CS and SS (may be this is disbonding).  UT for the plates was performed at the mill manufacturer as per SA 578 LEVEL B and it was acceptable.

Material is clad plate of thickness 20 mm (17 mm SA516 GR 70 + 3mm SS 316L).

Construction code is – ASME SEC VIII DIV1

Please inform whether any disbonding is acceptable as per code.

Please suggest whether above indication can be accepted on what basis. Please give code reference.

 

Thanks and Regards

Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...