Dear Vikas,
The ASTM/ASME equivalent of structural material S355J2+N is ASTM A572 Gr-50
Best Regards,
M.K.Choudhary
![]()
P.O. Box 877, Dammam 31421 KSA
Phone : (+9663) 8471840 X 555
Fax : (+9663) 8471291
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Arunachalam A
Sent: Tuesday, April 26, 2011 9:14 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:10867] ASME/ASTM equivalent of S355J2+N
It is NOT ASTM A36. A36 has specified tensile of 420 N/mm2.
On Tue, Apr 26, 2011 at 4:44 PM, SENTHILKUMAR SWAMINATHAN <skumarswami@yahoo.co.in> wrote:
Vikas,
Refer attached may help you. Hope it is A36 (ASTM)
Regards,
S.SENTHILKUMAR
From: Vikas Bhandari <vikas.bhandari349@gmail.com>
Sent: Tue, 26 April, 2011 9:09:50 AM
Subject: [MW:10855] ASME/ASTM equivalent of S355J2+N
Dear All
What is the ASTM/ASME equivalent of structural material S355J2+N (minimum yield strength 355 MPa, Tensile 470 to 630 MPa, C: 0.20 max, Si: 0.55 max, Mn: 1.60 max , CE: 0.45 max). A link to reference document stating the same would be much appreciated.
Thanks & best regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Arunachalam.A,
Abu Dhabi Gas Industries Ltd,
P.O.Box # 50124
Abu Dhabi, UAE
Mobile : +971-50-5257122
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments