[MW:10877] RE: 10751] Reduction in thickness-micro biological attack

Hello Anup,

MIC attack is very common in the industry. Would  you please elaborate on the scenario, e.g:- service, materials of construction and other aspects noted. MIC can be minimized a number of ways. Also reduction in pipe thickness could be alarming if it service is severe, and goes close to the required design thickness.

Feel free to get some basic information at this link:- http://events.nace.org/library/corrosion/Microbial/Introduction.asp

Thanks


Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of naik_anoop@rediffmail.com
Sent: Tuesday, April 19, 2011 11:49 PM
To: materials-welding@googlegroups.com
Subject: [MW:10751] Reduction in thickness

Can somebody give details on reduction in pipe thickness due to corrosion by micro biological attack.

Regards
Anoop naik

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...