Re: [MW:10824] usage of 45 deg elbow cut from 90 deg elbow.


45° Elbows are available as standard items. Why cut a 90° elbow?
In case you cut a 90° elbow to 45° - the 45° elbow here becomes a non standard item.


On Sun, Apr 24, 2011 at 7:15 AM, narasimha murthy <jnm71269@gmail.com> wrote:
Dear All,
 
Please suggest if you can cut a 90 deg elbow and use as 45 Deg elbow is it acceptable practice and if so is there any code refered to such usage.
 
Regards,
 
Murthy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...