[MW:10896] any acceptance standards availabe for structural steel? for fitup?

Dear all,

pl tell us..
Any acceptance standards for fitup & fabrication of structural steel..
Like welding codes AWS D1.1, ASME 9.
My client is not specified any codes..
& let me know any codes availabe for fitups like..
Type of joints & how much joints permitable in 6 meter..
type of inserts permitable..
Misalignment permitable..

Thanks & regards
m

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...