According to ASME sec IX, for GTAW, FCAW and GMAW in supplementary essential variables (QW 410.9) , a multi pass per side fillet/butt weld procedure cannot be used to weld single pass per side. (say single pass per side fillet weld.)
I am curious to know the technical reason behind the same. In my opinion, fill pass parameters of a butt weld procedure can be used for welding single pass fillet welds. Please advice if this is incorrect and kindly provide technical/ metallurgical reasoning for the same.
Thanks & best regards
-- To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments