Dear members,

Can any one give your suggestions on how to do a branch connections opening on Ti (Gr.2) header pipes. The max thickness of header is 6.35mm.
I mean what type of tools to be used to do the opening. Highly appreciate if any brand name suggested.

Rgds
Sudhakar

Sent from my iPhone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.