Molybdenum increases the resistance to pitting and crevice corrosion in Chloride environment. It supports the Chromium oxide layer and helps in re passivation, if the layer is broken


BR

On Tue, Nov 30, 2010 at 10:28 AM, Shiv Dutt Mishra Mishra <gopu301182@gmail.com> wrote:
Dear All,
Can you tell me what is the importance of '' MO"(molybdenum) content
in SS316L materials.

--
Thanks,
S.D.Mishra
Mob- 09589444897 (M.P./C.G.)
        09766916581 (Maharastra)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...