Sunday, November 28, 2010

Re: [MW:8416] SS 304 to SS 321 welding

308L is ok for dissimilar weld of this combination
genearally major alloying elements composition is same for both except 321 is stabilized steel,
kgp

On Thu, Nov 25, 2010 at 6:45 PM, <hrishikm07@gmail.com> wrote:
1.Pl advise if SS 304 to SS 321 piping welding is possible? If so what is the consumable to be used
2. Is welding of SS 321 possible with E 308 consumable provided one has an approved WPS/PQR?

Thanks
Hrishi
Sent on my BlackBerry® from Vodafone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...