Dear Majdi,
 
You didn't mention the material designation(pipe and split tee material) and thickness of the pipe/split tee material.If you could provide it,it will be easy for experts to analyse your query.I also have interest in this matter.
 
 
Regards,
 
Limesh

On Sun, Nov 28, 2010 at 6:45 PM, Majdi N Elyyan <melyyan@gmail.com> wrote:

Dear All;

 

We have a hot tap on LPG line (Sour service) which require PWHT.

The run Pipe is 4", the branch is also 4", split tee will be used.

As per shell DEP-31.38.60.10 – for Hot tapping, clearly mention:

Hot-tap welding should not normally be performed on materials which require post-weld

heat treatment. However, if stress relieving or post-weld heat treatment is required, a

specialist shall be consulted to assess whether it is feasible to make the specific

hot-tapping operation with post-weld heat treatment.

Note: Stress-relieving may be required if a material is susceptible to stress corrosion cracking and post-weld

heat treatment may be specified by the design code if the wall thickness is greater than a certain limit.

 

& since we have no other options, we have to do the hot tap on the same, kindly advice WPS & PWHT procedures

 

Thank all in advance..

 

Regards

Majdi Elyyan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...