Dear Mr.Praveen,
As per Indian Standard IS 3624,It is to be calibarated once in 3 months.
You can refer the customer or relevant applicable spec.
C.Muniyandi
Surveyor

On Thu, Nov 25, 2010 at 11:52 AM, Praveen Kumar <praveenkumar.sek@gmail.com> wrote:

Dear All,

 

Can you pls Suggest as the Piping Hydrotesting Pressure gauge calibration period of time,

and also is there any code/stds governing for this.

 

 

 

Regards,

 

Praveen Kumar

Mechanical Engineer

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...