Dear C.Nagabhushanam
 
Please find attached a WPS for a similar welding.
According to my experience for heavy pipes, preheat , clamping time  and time between passes can generate cracks, for instance during 4 first passes has not to be any movement of pipeline and time between them has to be short.
Let a joint only with three or four passes for finishing in the next day is take a risk of cracks. 
 
I'm not a native speaker, so pls excuse my english.
 
Regards
 

From: nagabhushanam@adorians.com
To: materials-welding@googlegroups.com
Subject: [MW:8400] Cracks in pipe wedling
Date: Sat, 27 Nov 2010 12:34:54 +0530

Dear ,

 

Please advise me for 34 inch Dia and 20mm thickness pipe of 65X why the cracks are observed while using E 8010G & remedial action.

 

Regards,

 

C.Nagabhushanam


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...