Re: [MW:8422] SA 316 - ASME 2A missing why?

316 is material grade, not standard. Based on end application, product form standard will be separate. For example, ASTM A666-Specification for stainless steel sheets which includes 316. ASME SA 240-Specification for SS plates, ASME SA312-Specification for SS Pipes.

2010/11/27 Srinivas Engr <srinivas.gmsrini@gmail.com>
Dear all

If i search in google, it ASTM 316 is a SS plate & bars.
But in ASME there is no such material grade........
Pl clear me....

Rgds
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...