Re: [MW:8402] Defect in PQR Specimen

Mechanical testing is carried out on a sample to find if the weld area / HAZ area meet the required/ declared mechanical properties. If you have to carry out a nick break test then this defect may be a prime reason for the sample not meeting the required mechanical properties which may eventually lead to rejecting the sample test results.


 
On Sat, Nov 27, 2010 at 10:00 AM, yoga nandhan <yoganandhan@gmail.com> wrote:
Anyone, Can u plz give your opinion,
 
PQR qualification of SS pipe, 30" x 15.88 mm thik pipe by SMAW+SAW process, In RT defect observed in 200 mm length which is not acceptable as per Sec IX. But rest of the portions are without any significant defects.
 
Can we proceed with the Mechanical testing after discarding the defect area or is it required to Repair & Re-RT to be done in the defect area before taking the specimen for mechancial testing.....  Plz clarify.
 
BR
P.Yoganandhan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Mohammad Afzal Baig
````````````````````````````````````````` email:afzal1972@gmail.com
        


  
     

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...