Greetings.
 
 
The total bevel angle for V JOINT for Butt weld is 60 Deg. Joint is category A type. Full Radiography is reuired for the joint.Construction code ASME SEC VIII DIV 1.
 
 
What will be the effect in terms of Design/Mechanical requiremnts if  the angle is reduced to 45 deg.
 
 
I mean if the total bevel angle is reduced to 45 deg( 15 deg less than the requirement) what will be the effect on  the joint.
 
also inform me what is the minimum total angle allowed for butt weld as per ASME SEC VIII DIV 1.
 
Thanks in advance for your valuable suggestions.
 
Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...