Rahul,

What's the design code? If it's ASME Sec-VIII,DIV-1, look under UNF. The attached booklet gives good information on various types of Titanium alloys. You may refer pages 5 through 10(both inclusive) for various design  and stress related values. However you need to verify the same from ASME Sec-II, Part-D for accuracy.

Best of Luck.

Thanks.


Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pisat, R. (Rahul)
Sent: Monday, November 22, 2010 7:29 AM
To: materials-welding@googlegroups.com
Subject: [MW:8350] P-T rating for Titanium Flanges

Dear All,

Has anyone calculated flanges for Titanium Piping ?
How can I approach a P-T rating ( for CL 150 & PN10 bar system ) for Titanium Flanges ( ie. Titanium Stub End and SS316 Lap Flange construction )

Waiting for your reply.

Rahul
____________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...