Sunday, October 31, 2010

Re: [MW:7952] DIN 62 FE Penetrameter Wire Range

IS THERE ANYTHING LIKE DIN 62 FE penetrameter?

--- On Sat, 30/10/10, Kale, Bhaskar M <bmkale@gmail.com> wrote:

From: Kale, Bhaskar M <bmkale@gmail.com>
Subject: Re: [MW:7938] DIN 62 FE Penetrameter Wire Range
To: materials-welding@googlegroups.com
Date: Saturday, 30 October, 2010, 2:14 PM

please see the attached file .DIN  and ISO IQI  wire diameter and number are same.

Bhaskar Kale
On Sat, Oct 30, 2010 at 4:08 PM, limesh M <limesh78@gmail.com> wrote:

Dear All,

How we can identify the number of wires(Range of wire like ISO penetrameter numbers 1-7,6-12,10-16) in DIN penetrameter?I have a RT film with DIN 62 FE penetrameter.What is the wire range of this penetrameter(To get the diameter of essential wire to calculate the sensitivity)?I have reference of all other penetrameters like EN,ISO and ASTM.Unfortunately,I am clueless about DIN.

EN wire type penetrameter(eg. 1 FE EN,6 FE EN etc.) and DIN wire type penetrameter are same or not?
 
Regards,
 
Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
धन्यवाद,
भास्कर मनोहर काळे
+60149129098

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...