Re: [MW:7931] Q235B equivalent

Steel Specification
ASTM A36  
ASTM A53 B
ASTM A106 B
ASTM A131 B
ASTM A139 B
ASTM A381 Y35
ASTM A500 A
  B
ASTM A501  
ASTM A516 55
60
ASTM A524
 
ASTM A529  
ASTM A570 30
  33
  36
  40
  45
ASTM A573 65
58
ASTM A709 36


On Fri, Oct 29, 2010 at 2:43 PM, Maroof Ali <maroofali.mohyuddin@gmail.com> wrote:
Dear friends

Chinese Q235B equivalent to which ASTM material?

Regards 

Maroof Ali

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...