--Yes, you can, provided all essential/supplementary essential variables are identical to original PQR.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of atul chaturvedi
Sent: Thursday, October 28, 2010 4:53 PM
To: materials-welding@googlegroups.com
Subject: [MW:0] Supporting PQR for Impact requirements
Dear All,
I have Qualified PQR for welding P1 Gr 1 To P1 Gr 1 with Impact test at (-) 51°C
thickness range 2.77 to 11.08 mm.
But now we have to weld P1 Gr 1 to P1 Gr 2. Can I do one more supporting PQR with with P1 Gr 1 to P1 Gr 2 With only impact testing.
Please clarify whether Tensile test and bend test are mandatory for supporting PQR.
Thanking you.
atul chaturvedi
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments