Dear Limesh, The wire IQI according to EN 462-1 are identical with the old DIN 54109 wire IQI. Wire etalons by the DIN 54109 standard Etalon number | Wire diameters, mm | 1-7 | 3.20 | 2,50 | 2,00 | 1,60 | 1,25 | 1,00 | 0,80 | 6-12 | 1,00 | 0,80 | 0,63 | 0,50 | 0,40 | 0,32 | 0,25 | 10-16 | 0,40 | 0,32 | 0,25 | 0,20 | 0,16 | 0,125 | 0,10 | --- On Sat, 10/30/10, limesh M <limesh78@gmail.com> wrote: From: limesh M <limesh78@gmail.com> Subject: [MW:7935] DIN 62 FE Penetrameter Wire Range To: "Materials & Welding" <materials-welding@googlegroups.com> Date: Saturday, October 30, 2010, 11:08 AM
How we can identify the number of wires(Range of wire like ISO penetrameter numbers 1-7,6-12,10-16) in DIN penetrameter?I have a RT film with DIN 62 FE penetrameter.What is the wire range of this penetrameter(To get the diameter of essential wire to calculate the sensitivity)?I have reference of all other penetrameters like EN,ISO and ASTM.Unfortunately,I am clueless about DIN.
EN wire type penetrameter(eg. 1 FE EN,6 FE EN etc.) and DIN wire type penetrameter are same or not? Regards, Limesh -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
| -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
|