[MW:7950] NAXTRA M700 weldebility

We are going to use above material fro shipbuilding purpose. Thickness 30- 40 mm. We do not have experience with this specified material, I would like to know from your experience information on ;
Ceq and impactvalue in L and T direction.
 
In regard to the attached manufacturers information , the deviation in chemical composition may be rather high.
 
This may require preheating, which influences the weldebility. If you have any practical information, it will be appreciated.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...