RE: [MW:7877] Group No for S 355 material in AWS D1.1

These are unassigned materials in AWS D1.1 (not sure if it is changed in the latest edition, pl check?)

 

If these pile are manufactured to API 2B, the max straightness can be computed with the following formula

 

1/8”  x total length in ft/10 ft, but not to exceed 3/8” in any 40 ft length.

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of muthu barathi
Sent: Wednesday, October 27, 2010 6:28 PM
To: materials-welding@googlegroups.com
Subject: [MW:7875] group no

 

Hi All Friends,

I want to make proposed WPS as per AWS D 1.1 - 2006 for material BS EN
10025 - 1993grade S 355 JO (for Pile splice fabrication dia 900mm and
1200mm and thickness 22mm and structural fabrication material grade is S
235 JR.

Also what is the tolerance for straightness of Pile . Pile length will
be 60 meter of 12meter joint.

Please suggest group no for the given materials.

Thank you all.

Dear Sir,

Thanking You,

Honesty is the best Policy

With Warm Regards,

P Muthu Barathi
Mobile No:09967300544

 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...