Friday, October 29, 2010

Re: [MW:7928] Q235B equivalent

Hi,


Equivalent to CHINA STEEL STANDARDS - Q235B are as below


DIN17100-80 - St37-2


EN10025-2:1998 -  S235JR 


ASTM - A283 


JIS - SM400A


Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 10/29/10, Maroof Ali <maroofali.mohyuddin@gmail.com> wrote:

From: Maroof Ali <maroofali.mohyuddin@gmail.com>
Subject: [MW:7926] Q235B equivalent
To: materials-welding@googlegroups.com
Date: Friday, October 29, 2010, 1:43 PM

Dear friends

Chinese Q235B equivalent to which ASTM material?

Regards 

Maroof Ali
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...