Re: [MW:7895] Re: WQT-Visual Acceptance Criteria Issue

Dear Mr. Robert,
 
Thank you for the valuable inputs. I reviewed ASME B31.3 Chapter 5 & 6 and observed the following things
 

328.2 Welding Qualifications

328.2.1 Qualification Requirements

(a)

Qualification of thewelding procedures to be used and of the performance of welders and welding operators shall conform to the requirements of the BPV         Code,Section IX except as modified herein.
 
341.4.2 Examination — Category D Fluid Service.

Piping and piping elements for CategoryDFluid Serviceas designated in the engineering design shall be visually examined in accordance with para. 344.2 to the extent necessary to satisfy the examiner that components, materials, and workmanship conform to the requirements of this Code and the engineering design. Acceptance criteria are as stated in para. 341.3.2 and in Table 341.3.2, for Category D fluid service, unless otherwise specified.

 

 

 

Criterion Value Notes for Table 341.3.2

 

C                 Depth of lack of fusion and incomplete penetration                      0.2T w

                          Cumulative length of lack of fusion and incomplete                          38 mm (1.5 in.) in any 150 mm (6 in.) weld length

                          penetration [Note (7)]

 

 

                           Note (7) Tightly butted unfused root faces are unacceptable.

 

Mr. Robert, Suppose my company's scope of work comes under category 'D' fluid service. As per B31.3 Table 341.3.2, lack of fusion and penetration is acceptable up to some extend for girth and miter groove!!! But ASME SEC IX says complete fusion and penetration required during WQT (irrespective of fluid service).  Can I qualify my welders with ASME B31.3 visual acceptance criteria for category 'D' fluid service?

 
 
 
Regards,
 
 
Limesh

 

 

On Wed, Oct 27, 2010 at 9:37 PM, <robertp@westernp.com> wrote:
Sec IX is not BPV Code, it is reference book for qualification
requirements.

Refer to VT in chapt 6 of B31.3 process piping code.

On Oct 26, 9:33 pm, limesh M <limes...@gmail.com> wrote:
> *Dear All,*
> **
> *Design Code - ASME B31.3*
> *Welding Code - ASME BPV SEC IX*
> **
> *I want to qualify some welders and welding operators based on ASME BPV SEC
> IX.*
> *What is the visual acceptance criteria as per code (Suppose there is no
> client specification regarding this matter)?*
> *Please mention the relevant code clauses for reference.*
> **
> **
> **
> **
> *Regards,*
> **
> **
> *Limesh*

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...