Re: [MW:6780] 9Cr-1Mo/9Cr-1Mo-V steel welds

Hi Abby

Pls note that , 9Cr-1Mo/9Cr-1Mo-V Steels are the Ferritic Steels.

Don't confuse Sigma embitterment of ASS with Ferritic Steels.

Regards,

K.Babu
Singapore


----- Original Message -----
From: "Abby Joseph" <abbyjoseph@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Sent: Monday, August 30, 2010 4:37 PM
Subject: [MW:6775] 9Cr-1Mo/9Cr-1Mo-V steel welds


> Do 9Cr-1Mo/9Cr-1Mo-V steel welds also develop sigma phase during
> service, like some stainless steels?
> (Note- these alloys also contain substantial wt% of Cr, Fe and Mo.
> They are also exposed to the high temp at which sigma phase forms.)
> If not, why?
>
> Regards,
>
> Abby Joseph
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...