RE: [MW:6723] Opening on long seam welding

Any type of opening that meets the requirements for reinforcement given in UG-37 or UG-39 may be located in a welded joint (refer UW14)


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of waman nilesh
Sent: Wednesday, August 25, 2010 9:18 PM
To: materials-welding@googlegroups.com; materials-welding@goolegroups.com
Subject: [MW:6712] Opening on long seam welding

Dear All,
 I want to know  is it allow opening on Long seam of Head ( Dish end ).
Job- Pressure Vessel ( Tank )
Design- ASME Sect.-VIII Div.-I
Pressure- 1.3 bar 
Thickness of Head - 6 mm
And where did i get reference.

With Regards,
Nilesh Waman