All asme bpvc sections require pwht for p91


  From: "Mohamed Farook" [asfaruk@gmail.com]
  Sent: 30/08/2010 12:00 ZE8
  To: <materials-welding@googlegroups.com>
  Subject: [MW:6769] Any WPS for P91 Material without PWHT


Dear friends,

 

Greetings to all,

 

Please advise me if you have WPS for P91 material without PWHT….

 

PWHT is time consuming..

 

Thanks and Regards,

asfaruk

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...