[MW:0] RE: 6716] Charpy Test

 

 

 

You can just weld the additional test copon using the existing wps parameters

John du Plessis

Technology Manager

 

Tel: +27 (11) 298 2100

Tel: +27 (11) 298 2103 (Direct)

Fax: +27 (11) 836 6014

Mobile:+27  82 883 4970

www.saiw.co.za

 

This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Larry
Sent: 26 August 2010 02:01 AM
To: materials-welding@googlegroups.com
Subject: [MW:6716] Charpy Test

 

Hi There,

 

We have an existing WPS, The existing WPS doesn’t have a cold service specification, and we would like to do a test coupon from that WPS and have it charpy tested, so we can revised the existing WPS. Now the requirement of the client is -70 degrees Celsius. Is that alright or do we have to do another PQR? Code is ASME IX.

 

 

Thank you,

 

Larry Zarate