Tuesday, August 31, 2010

RE: [MW:6796] Propane or butane to preheat

Nothing wrong in it, gas used for heating is not a variable to consider.

sent from my handheld
-----Original Message-----
From: eduardocalva@hotmail.com
Sent: 31/08/2010 12:00:40 am
Subject: [MW:6794] Propane or butane to preheat

Could all of you tell me the difference between preheat with propane
and butane?, If a WPS is qualified by preheating with propane but
butane is used in production welds is wrong?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...