[MW:6746] Re: Pressure vessel in Austenitic-Ferritic Stainless Steel

Dear Mr. Raghuram,

Grade was not known by me right know, I needed to find a alternative
for 1.4462. But with the specification mentioned by you I find out
that UNS 32205 is the alloy we need to specify in our purchase order.
I only have a copy available of the 2007 edition of ASME, what is your
opinion can I still use this or do I really have find a copy of the
2010 version?

Best Regards,

Herman Pieper

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...