Hi Shashank,
 
Thanks for attachment.
I found on it the T23 filler metal for 2.25Cr-1Mo. I will make a comparison between it and others that Pgoswami has suggested.
 
Thanks for your interest Shashank.
 
L. Carlos Flores
Piping Team Leader
Oficina:(993) 310 8100 Ext. 106
Celular:(993) 250 6610



 



Date: Tue, 31 Aug 2010 05:24:01 +0530
From: nach_sam@yahoo.com
Subject: Re: [MW:6791] A 217 Gr WC9
To: materials-welding@googlegroups.com

Hi Luis,
I hope the attached Bohler data sheet will be useful. Please let me know if you found in it what you looked for.
Thanks,
Shashank Vagal

--- On Mon, 30/8/10, Luis Carlos <carlosflores126@hotmail.com> wrote:

From: Luis Carlos <carlosflores126@hotmail.com>
Subject: [MW:6788] A 217 Gr WC9
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Monday, 30 August, 2010, 10:06 PM

Hello,

Could someone tell me please what is the best filler metal to make a
buttering over A-217 Gr WC9 base metal.

Are there special recommendations?

I will appreciate answers!

Luis Carlos

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...