Hi,
         If we don't have any client specification, where can we get this type general detail. Is there any book for general engineering practice?
 
Louis


From: B.Vaithiyanathan <pavainathan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, 13 June, 2010 11:48:55 PM
Subject: Re: [MW:5577] Distance between welds

Hi
 this is for your info
One of my client specification allows the Minimum distance between(toe to toe) weld can be 5 times the wall thickness provided both joint can be radiographicaly acceptable.If in case of sour service Hardness check on weld ,HAZ & Base metal is required.
 
vaithiyanathan

On Sat, Jun 12, 2010 at 10:17 AM, manpreet <manpreetsin88@rediffmail.com> wrote:
Dear All

My case is:-

code of construction- ASME B31.3
LPG/LNG pipeline

For Pig signaller, we have to weld a barred tee in the pup piece attached with valve.

pup piece material- API 5L X60 PSL2
barred tee- ASTM A860 WPHY 60

length of pup piece is 125 mm. Kindly find the attached drawing for welding connection.

Acc. to Australian std distance between welds should be 6 times of thickness, in this case we r not able to weld.
PLS confirm looking at the drawing, can the welding be performed?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...