Wednesday, June 30, 2010

Re: [MW:5809] P1 to P8 group metal joining

In welding Type 304 to mild steel for instance, the choice of filler metal is a key point. If you use Type E308 filler metal, the diluted weld metal with the formation of martensite (a brittle structure) may contain cracking, because the filler metal cannot tolerate dilution by both base metals. A proper filler metal, in this case, is Type E309 (typically contains 24% Cr and 13% Ni.), for applications below 315 deg C in general. The procedure of estimating the micro structure of the E309-type diluted weld metal can be done by using a Schaeffler diagram ; the diluted weld metal will contain about 4% of ferrite and no martensite in the austenitic matrix, which is resistible to cracking

On Wed, Jun 30, 2010 at 6:57 PM, limesh M <limesh78@gmail.com> wrote:
Dear All

What would be the problem if we use E 308L electrode instead of E 309L
to join P1 to P8 dissimilar material joining in oilfield sour service?
On what basis we are selecting E 309 L over E 308 L in P1 to P8
dissimilar metal joining?

Thanks and Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...