Generaly you can demagnetize by 2 ways that what I know
1- preheating
2- rotate the welding cable around the tube with high current.
best reggads
 
Tamer Said
 
--- On Wed, 6/23/10, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:

From: Muhammed Ibrahim PK <ibratech@gmail.com>
Subject: [MW:5720] How to demagnetise the tube sheet?
To: materials-welding@googlegroups.com
Date: Wednesday, June 23, 2010, 12:48 PM

Hi Members,
 
We are suffering a problem in tube sheet. The tube sheet is P5A material (SA 336 Gr F22 CL.3) is magnetised.
 
We are not able to proceed the GTAW welding of tube to tube sheet.
 
We are not sure how it is happened. How can we demagnetise the tube sheet.
 
It is around 275 mm Thk and 3 mtr dia.
 
Kindly request the solution from experts.

Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...