Thursday, June 24, 2010

[MW:5732] Urea reactor lining repair

Dear Mr. Prabhu Kumar,

 

We are using ER Thermanit 19/15H for restoration of lining welds of our Snamprogetti Urea reactor. Material of lining is 316-L (mod) Urea grade. But after one year of service the repaired welds again undergo erosion/corrosion. Can we use ER Thermanit 25/22H instead, for a better life of repaired welds?

 

 

Regards,

 

Mahmood

 

 

 

 

 