Dear Mr.Vijay,
 
As per ASTM A 320 sec 9 it is clearly mentioned that nuts to be of ASTM A 194 Grade 4 or Grade 7. Please refer the below.

9. Nuts and Washers

9.1 Bolts, studs, and stud bolts of Grades L7, L7A, L7B,

L7C, L43, L1, L70, L71, L72, and L73 shall be equipped with

ferritic alloy nuts conforming to Grade 4 or Grade 7 of

Specification A 194/A 194M or a grade of steel similar to the

studs. Grade 7M nuts at a hardness not exceeding 235 HB (or


regards,
On Tue, Jun 29, 2010 at 10:14 AM, Vijay <k.vijayaraj@gmail.com> wrote:
Dear All,

For one of our project the fastener requirement was LTCS material as
per project Specification.

The Bolts we received were ASTM A320 Gr. L7 but Nuts we received were
ASTM A194 Gr. 2H

Whether is it is acceptable ????

Kindly clarify.

Regards,
Vijay.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
G.Murali krishnan
Saudi Arabia


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...