Wednesday, June 30, 2010

[MW:5806] P1 to P8 group metal joining

Dear All

What would be the problem if we use E 308L electrode instead of E 309L
to join P1 to P8 dissimilar material joining in oilfield sour service?
On what basis we are selecting E 309 L over E 308 L in P1 to P8
dissimilar metal joining?

Thanks and Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.