[MW:5746] Calibration of welding Measuring Instruments

Dear All,
 
Please advice me whether calibration is required for welding measuring gauges like BRIDGECAM, HI-LOW GAUGES , FILLET GAUGES & etc, if so what is the frequency of calibration and please mention the reference standard.
--
G.Murali krishnan
Saudi Arabia

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.