Wednesday, June 30, 2010

[MW:5801] NPC Approved Stainless Steels Castings


Can some one Help me on...
  • (A) ASME Section 3NC-2573, ASME Section 2SA-613
  • (B) Soundness is to be 51mm Severity level 2 as per ASTM E446 / E186 Delta ferrite %5 for Stainless Steels


Regards
P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...