[MW:3047] RE: 3038] G4859 (suitable consumables for 800H)

I don't know exact properties of G4859, however based on the nominal
composition given; it seems suitable consumables can be
ERNiCr-3, ERNiCrCoMo-1, ENiCrFe-2, ENiCrCoMo-1 etc.


-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Siva Shanmugam
Sent: Thursday, August 27, 2009 6:36 PM
To: Materials & Welding
Subject: [MW:3038] G4859


Dear All,
I would like to know the filler material for G4859(20cr32ni 1nb P.no.
45) reformer catalyst tube reducers with pigtail tube UNS 08810.
Expecting the all of them suggestions.

Best regards,
R.Sivashanmugam.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...