Dear Sir Bottom Plate we have more distortion , what
is
the tolerance and how to measure.Tank dia 72m, API 650,Thk 9mm,height
20m,Methanol Tank.
is
the tolerance and how to measure.Tank dia 72m, API 650,Thk 9mm,height
20m,Methanol Tank.
Regards
suresh kumar
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---