Thursday, August 27, 2009

[MW:3040] Re: Bottom plate tolerance of Tank.

 
 Dear Friend,
 
The distortion is like bulge or depression ,you can refer API 653 AppendixB 3.3


--- On Wed, 26/8/09, bdsathiyamoorthy <bdsathiyamoorthy@gmail.com> wrote:

From: bdsathiyamoorthy <bdsathiyamoorthy@gmail.com>
Subject: [MW:3030] Bottom plate tolerance of Tank.
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, 26 August, 2009, 11:59 PM


Dear All,
Pls any one can suggest to me that  We are using API 650 (Year 2005)
tank fabrication, Now the problem bottom plate distration tolerance
not able to get from  API 650. Kindly I request to all  please any one
can suggest to me what is the tolerance of bottom plate distration.

Thanks in advance,


Love Cricket? Check out live scores, photos, video highlights and more. Click here
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...