[MW:3061] Re: piping and pipleine spacing

Dear Daniel ,
 
If you are looking for spacing between the pipe and the ground , it is stated in the API 1104 for p/l ,
 
If you are looking for spacing between 2 welds  usually it is 3  times diameter , or as per client specification
 
Usually this is defined as if the lenght is less will cause distorsion if the pup piec is very small in lenght and at the same should see their is a min spacing of 2 " between the HAZ of the 2 welds , in case u need to come to a smaller lenght .
 
Thanks
 
Sujeet
On Fri, Aug 28, 2009 at 12:48 PM, daniel iordache <daniel.iordache@gmail.com> wrote:

dear all,

i have 3 pipeline burried ...i need to know what minimum spacing is
recommanded....(api 1104/ b31.4)

thanks

regards

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...