Hi,
 
There is no difference between the both the spec.
 
But , the De -Oxidation practice is different in steel making  . ie API 5L Gr.B is non-silicon killed steel,, and ASTM A106 Gr.B is silicon killed steel.
 
Obviously , the ASTM A106 Gr.B will have comparatively higher corrosion resistance .
 


 
On Fri, Aug 28, 2009 at 2:51 AM, sohaib.t <sohaib_cegco@yahoo.com> wrote:


Gentlemen,

is there any difference between the welding procedures of API 5L GR.B
and ASTM A106 GR.B?

Regards,

Sohaib



Thanks & regards,

   K.Babu
   Singapore



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...