[MW:3036] TGX Welding

Dear All,

TGX Welding (root pass welding with out back purging) possible to use
the same filler wire to weld hot pass?
Also it is adviseble to use SMAW after root pass?

Please can any one suggest the pass sequence for TGX Welding.

Thanks in advance

Regards,
Pugal

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS