Dear sandeep
these are wiki links for better understanding
http://en.wikipedia.org/wiki/Curie_temperature
http://en.wikipedia.org/wiki/Magnetic_domain
--
Best Regards;
ASIF IQBAL SYED
CSWIP 3.1-38557,
ASNT-Level II (RT, UT, MPT & LPT)
0091-99750 163 55
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
these are wiki links for better understanding
http://en.wikipedia.org/wiki/Curie_temperature
http://en.wikipedia.org/wiki/Magnetic_domain
--
Best Regards;
ASIF IQBAL SYED
CSWIP 3.1-38557,
ASNT-Level II (RT, UT, MPT & LPT)
0091-99750 163 55
On Fri, Aug 7, 2009 at 10:49 AM, sandy kumar <sandy001987@gmail.com> wrote:
Why Austetic steel is non-magnetic as compare to martenstic steel?e.g. in austentic steel main constitute are Iron+chromium+Nickel & in martentstic steel main constitute are Iron+chrmium.There is addition of nickel in Austentic steel, but nickel is a feroomagetic material how it make the autentic steel non-magnetic?Please tellRegardsSandeep Kumar
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments