[MW:3049] Re: API 5L GR.B & ASTM A106 GR.B

Dear Sohaib,
 
It will depend on the code you are using is yourexisting procedure has the same code as to the new one you intend to use.
 
Does it cover the thickness and Diameter range
 
As per AWS D 1:1 they come is same group
 
As per ASME Sex IX , they have same Group No. 1 .
 
They have the same strenght 60 Ksi - Tensile strenght .
 
You have to see if any additional Test is required i.e Impact or Corrosion test by the client Spec. as to the previous
 
If all are matching need to check the Electrode Batch or need to contuct the batch test .
 
Let me know if any more information is required or it covers your query .
 
Thanks
 
Sujeet
On Fri, Aug 28, 2009 at 12:21 AM, sohaib.t <sohaib_cegco@yahoo.com> wrote:


Gentlemen,

is there any difference between the welding procedures of API 5L GR.B
and ASTM A106 GR.B?

Regards,

Sohaib




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...